Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 860 MPa @Strain 0.200 % |
>= 125000 psi @Strain 0.200 % |
H1075 Condition - 580°C at 4 hr |
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Tensile Strength, Yield | 860 MPa @Strain 0.200 %, Temperature 540 °C |
125000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Tensile Strength, Yield | 862 MPa @Temperature -55.0 °C |
125000 psi @Temperature -67.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
H1150 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
H1150 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
H1150 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
Tempering Temperature-1200°F |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |