Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 186 MPa @Strain 1.00 %, Temperature 200 °C |
27000 psi @Strain 1.00 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 23.0 °C |
27000 psi @Temperature 73.4 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 23.0 °C |
27000 psi @Temperature 73.4 °F |
Conditioned; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 23.0 °C |
27000 psi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 23.0 °C |
27000 psi @Temperature 73.4 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Strength, Yield | 186 - 262 MPa @Strain 0.200 % |
27000 - 38000 psi @Strain 0.200 % |
Annealed, Transverse Orientation, 0.05"-0.085" |
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Yield | 186 MPa @Temperature 649 °C |
27000 psi @Temperature 1200 °F |
Vacuum |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |