Polymer Property : Flexural Modulus, 1% Secant = 900 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM D790A
SABIC PP 651H Polypropylene Random Copolymer for PIPE
Product Description: PP 651H is specially designed for transport of hot and cold drinking water. This grade is highly heat stabilized and specially formulated for extraction resistance.Typical App..
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer
PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive..
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer
PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. ..
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Braskem PRB 0131 RACO Random Polypropylene Copolymer
PRB 0131 is a low melt flow rate random copolymer with high transparency. This resin is designed for thermoforming, blow molding, and extrusion. This product exhibits excellent processability, low h..
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Braskem Prisma 2400 RACO Random Polypropylene Copolymer
Prisma 2400 is a high melt flow rate random copolymer. This product is designed for the ISBM (Injection Stretch Blow Molding) process and offers low taste/odor. It can also be used in the blow moldi..
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM D790A
Braskem CP 741 Extrusion Polypropylene Heterophasic Copolymer
Sheet extrusion.Information provided by Braskem.