Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature 0.000 °C
22.4 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East)
XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East)
XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi..
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -20.0 °C
22.4 ft-lb/in²

@Temperature -4.00 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® CL402U PBT+PC (Europe-Africa-Middle East)
XENOY CL402U has been specially developed for extrusion blowmoulding applications, where higher melt strength is desired. XENOY CL402U is a high impact material combined with good UV resistance perf..
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature 0.000 °C
22.4 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature 0.000 °C
22.4 ft-lb/in²

@Temperature 32.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180-4A
Styron Pulse® 2000EZ PC/ABS
Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Izod Impact, Notched (ISO) 47.0 kJ/m²

@Temperature -30.0 °C
22.4 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
Styron PULSEâ„¢ 2000 EZ PC/ABS Engineering Resin
Overview: PULSE 2000 Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can wi..
Copyright © lookpolymers.com All Rights Reserved