Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -40.0 °C
1.19 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66  (Unverified Data**)
Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66  (Unverified Data**)
Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -40.0 °C
1.19 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified ..
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Domo 1040RC Polypropylene Homopolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 2300K Polypropylene Copolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 2300L Polypropylene Copolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 2340P Polypropylene Copolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Domo 2348M Polypropylene Copolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -30.0 °C
1.19 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecolen® HP30 NL XA80 PPHP, flame retardant, halogen free, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Domo 1040N Polypropylene Homopolymer
Information provided by Domo.
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry)
Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF
Izod Impact, Notched (ISO) 2.50 kJ/m²

@Temperature -10.0 °C
1.19 ft-lb/in²

@Temperature 14.0 °F
ISO 180
LyondellBasell Hostacom™ ZB752AC Polypropylene Homopolymer