Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2783 |
ExxonMobil 24 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2596 |
ExxonMobil Unirex S 2 Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2596, DIN 51 350/4 |
Chesterton 601 Chain Drive Pin & Bushing Lubricant Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | kgf; ASTM D2783 |
ChevronTexaco Pinnacle® 220 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | kgf; ASTM D2783 |
ChevronTexaco Pinnacle® 680 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2596 |
ExxonMobil Unirex S 2 Unirex S 2 is premium-quality high-temperature grease, based on a low volatility, synthetic polyol ester fluid, thickened with a lithium complex soap thickener, and containing performance-enhancing .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6068 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6220 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6320 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6460 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6680 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 15 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 150 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 460 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2783 |
ExxonMobil 24 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 68 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 10 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | |
ConocoPhillips Hydroclear® 320 Rolling Oil Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary addi.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | kgf; ASTM D2783 |
ChevronTexaco Pinnacle® 320 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | kgf; ASTM D2783 |
ChevronTexaco Pinnacle® 460 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D-2783 |
ConocoPhillips ANDEROL® 6150 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Four Ball Extreme Pressure, Weld Load | 160 kg | 353 lb (mass) | ASTM D2266, DIN 51 350 |
Chesterton 652 Pneumatic Lubricant & Conditioner Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e.. |