Material Notes:
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide outstanding stability resulting in longer lubricant and equipment life.Extended machinery life and increased compressor efficiency — Oxidative stability and low carbon-forming tendencies minimize sludge and deposit formationExtended drain intervals — Longer lubricant life means less frequent oil changes.High viscosity index and low pour point — These result in very broad operating temperature ranges -46°C to 149°C (-50°F to 300°F) when compared with conventional mineral oil based lubricants.Reduced oil consumption — Low volatility means less oil goes downstream, and less oil is needed for makeup.Reduced maintenance and downtime — Trouble free operation and extended service intervals means reduced operating costs.Excellent thermal and oxidation stability — Reduces the formation of oxidation byproducts and acidic materials which cause deposits and varnish.Texaco Pinnacle oils are synthetic circulating/non-EP bearing and gear lubricants. They provide:Excellent thermal and oxidation stabilityHigh viscosity indexHigh flash pointLow pour pointExcellent hydrolytic stabilityTexaco Pinnacle oils:Are able to withstand relatively high temperature operations for extended periods of timeHave very good demulsibility characteristics allowing quick release of moistureMinimize entrained air, which could result in reduced lubricant film thickness and potentially lead to pump cavitation.Texaco Pinnacle oils are formulated to provide outstanding lubrication qualities for air compressors, especially portable and stationary rotary, vane and screw compressors.Texaco Pinnacle oils are recommended for industrial bearings and gears, such as worm gears, that require an R&O type synthetic gear oil.Texaco Pinnacle oils are designed for applications with wide operating temperature ranges. They are especially effective in high temperature applications, like sootblowers, where outstanding thermal and oxidative stability are required. Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.Do not use in breathing air apparatus or medical equipment.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 222097; MSDS Number: 8983
Physical Properties Metric English Comments
API Gravity 32.4 °
32.4 °
Viscosity Measurement 147
147
Viscosity Index
Saybolt Viscosity at 100°F 1081 SUS
1081 SUS
Saybolt Viscosity at 210°F 121 SUS
121 SUS
Kinematic Viscosity at 40°C (104°F) 209 cSt
209 cSt
Kinematic Viscosity at 100°C (212°F) 24.6 cSt
24.6 cSt
Oxidative Stability 16.67 hour
16.67 hour
to 25 psi drop; ASTM D2272
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
kgf; ASTM D2783
Thermal Properties Metric English Comments
Pour Point -31.0 °C
-23.8 °F
Flash Point 270 °C
518 °F