ConocoPhillips Hydroclear® 150 Rolling Oil

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 150 Rolling Oil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Conoco Hydroclear Rolling Oil is a multipurpose rolling oil formulated from premium Conoco hydrocracked base stocks. Hydroclear Rolling Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of rolling applications for nonferrous materials, such as aluminum, copper, brass and other copper alloys. Hydroclear Rolling Oil is nonstaining, does not contain zinc and provides very good wear protection for use in hydraulic systems. Hydroclear Rolling Oil also can be used as an exceptional bearing lubricant and as a roll-coating oil in most mill applications. Hydroclear Rolling Oil provides exceptional oxidation resistance, foam control, rust and corrosion protection and rapid low-temperature demulsibility. Hydroclear Rolling Oil exceeds the performance requirements of Vickers I-286-S and U.S. Steel 127 and 136. Hydroclear Rolling Oil in ISO viscosity grades 150, 320 and 460 exceeds the Morgan Construction Company lubricant specifications for use in No-Twist Rod Mills.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.877 g/cc
0.0317 lb/in³
Viscosity Measurement 100
100
Viscosity Index
Saybolt Viscosity at 100°F 786 SUS
786 SUS
Saybolt Viscosity at 210°F 80 SUS
80 SUS
Kinematic Viscosity at 40°C (104°F) 150 cSt
150 cSt
Kinematic Viscosity at 100°C (212°F) 15.1 cSt
15.1 cSt
Oxidative Stability 5000 hour
5000 hour
ASTM D 943
ASTM Color 3.0
3.0
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 160 kg
353 lb (mass)
Four Ball Wear 0.420 mm
0.0165 in
Thermal Properties Metric English Comments
Pour Point -28.9 °C
-20.0 °F
Rotating Bomb Oxidation Test (RBOT) 600 min
600 min
ASTM D 2272
Flash Point 260 °C
500 °F
Descriptive Properties Value Comments
ASTM Rust A&B Pass
ASTM D665
Copper Corrosion 1A
Emulsion Characteristics (40-40-0) 15 minutes
Foam Control (Sequence I,II,III) 0-0-0
FZG Pass 12 Load Stages
ASTM D5182