Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.Avail.. |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² | 3.90 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **) Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg.. |