Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 43.0 kJ/m² | 20.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² | 20.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® 4251R PPC+PC High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² | 20.5 ft-lb/in² | ISO 180 |
MRC Polymers MAXTEL™ 620-BK Polypropylene Copolymer • For injection molding• Excellent process ability with high flow and high impact.Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² | 20.5 ft-lb/in² | ISO 180-1A |
Gromax BTE45-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC LNP* LUBRILOY* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, High Impact. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific) LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CE PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00CE is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 (Asia Pacific) LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² | 20.5 ft-lb/in² | ISO 180/4A |
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant High Heat |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Izod Impact, Notched (ISO) | 43.0 kJ/m² @Temperature -40.0 °C |
20.5 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RX06424 PA 66 LNP VERTON* RX06424 is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural |