Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.70 - 13.0 kJ/m² | 1.76 - 6.19 ft-lb/in² | Average value: 10.1 kJ/m² Grade Count:20 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Izod Impact, Notched (ISO) | 3.70 kJ/m² @Temperature 23.0 °C |
1.76 ft-lb/in² @Temperature 73.4 °F |
ASTM D256 |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Izod Impact, Notched (ISO) | 3.70 - 17.0 kJ/m² | 1.76 - 8.09 ft-lb/in² | Average value: 11.3 kJ/m² Grade Count:11 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched (ISO) | 3.70 kJ/m² | 1.76 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ S 218 MZ20 V10 Black 2N PA6, 20% mineral, 10% glass filled, DRY Description: TECHNYL STAR Polyamide, 20% mineral filled and 10% of glass fiber reinforced, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe a.. |
|||
Izod Impact, Notched (ISO) | >= 3.70 kJ/m² | >= 1.76 ft-lb/in² | DIN 53453 |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Dry Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 3.70 kJ/m² | 1.76 ft-lb/in² | ISO 180 |
Polyram PlusTek PA340S4 Nylon 66 for Injection Molding, 20% Glass-Beads Reinforced 20% Glass-beads reinforced Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 3.70 kJ/m² | 1.76 ft-lb/in² | ISO 180 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched (ISO) | 3.70 kJ/m² | 1.76 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NCHA Homopolymer 25% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Notched (ISO) | 3.70 - 4.70 kJ/m² @Temperature -40.0 - -40.0 °C |
1.76 - 2.24 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 4.03 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |