Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature 23.0 °C |
1.67 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**) Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO Test |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ASTM D256 |
Tipco Tipcolene® FPT 20 - 20% Talc Reinforced Polypropylene Homopolymer Compound 20% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® FR1841-BK1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180 |
Total PPH 4069 Polypropylene Homopolymer, Fiber Polypropylene PPH 4069 is a homopolymer polypropylene with a Melt Flow index of 4 g/10 min.Polypropylene PPH 4069 is intended for extrusion of high tenacity staple fibers for non-woven applications... |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 7069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9081 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9081 is a controlled-rheology homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing improved impact res.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 179 |
Total PPH 9099 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9099 is a very narrow molecular weight distribution homopolymer polypropylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9099 is intended for.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IIQ Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IR Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: High-voltage insulation material at mains frequency. High breakdown voltage in oil and reasonable breakdown voltage in air at normal air humidity. Very low water absorption.Application:.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin 6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont .. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | DAM; ISO 180/1A |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 ZG30 Nylon 6, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2 G30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Temperature -20.0 °C |
1.67 ft-lb/in² @Temperature -4.00 °F |
ASTM D256 |
C.O.I.M. LARIPUR® LPR72D25 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² | 1.67 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2H G15 Flame Retardant Nylon 6, 15% Glass Bead Flame retardant, 15% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.50 kJ/m² @Thickness >=5.00 mm |
1.67 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit 201M S Phenolic, Paper Reinforcement, Black, Sheets Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications. The material is black throughout. Used where the mecha.. |