Polymer Property : Izod Impact, Notched (ISO) = 75.0 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East)
LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East)
LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EX1332T PC (Europe-Africa-Middle East)
LEXAN* EX1332T polycarbonate resin, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP6NR PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP6REU PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East)
Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7 PC (Europe-Africa-Middle East)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7R PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7R PC (Asia Pacific)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® PK2870 PC
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific)
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East)
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EX1632T PC (Europe-Africa-Middle East)
LEXAN* EX1632T polycarbonate resin, MVR (300C/1.2kg) 6 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP6NR PC
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7 PC
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPS7 PC (Asia Pacific)
Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP COLORCOMP DX04401H PC
LNP* COLORCOMP* DX04401H is an unfilled Polycarbonate. Added feature of this grade is: Healthcare.
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® C 216 PA6, Conditioned
Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel..
Izod Impact, Notched (ISO) 75.0 kJ/m²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ 2091-15 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARADâ„¢ 2091 Polycarbonate Resins are designed for single use medical devices (SUDs) that require gamma and electron-beam irradiation and an accelerated schedule for de..
Izod Impact, Notched (ISO) 75.0 kJ/m²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi..
Izod Impact, Notched (ISO) 75.0 kJ/m²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Styron CALIBREâ„¢ MEGARAD 2081-HD-15 2 Polycarbonate Resin
Overview: CALIBREâ„¢ MEGARAD 2081 HD-15 2 polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed ..
Izod Impact, Notched (ISO) 75.0 kJ/m²
35.7 ft-lb/in²
ISO 180/4A
Chi Mei Wonderlite® PC-115 Polycarbonate
Low Viscosity