Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 23.0 - 45.0 kJ/m² | 10.9 - 21.4 ft-lb/in² | Average value: 36.5 kJ/m² Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Izod Impact, Unnotched (ISO) | 32.0 - 45.0 kJ/m² | 15.2 - 21.4 ft-lb/in² | Average value: 40.7 kJ/m² Grade Count:3 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 45.0 kJ/m² | 9.52 - 21.4 ft-lb/in² | Average value: 26.3 kJ/m² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 45.0 kJ/m² @Temperature -30.0 - -30.0 °C |
19.0 - 21.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 41.3 kJ/m² Grade Count:4 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 45.0 kJ/m² | 16.7 - 21.4 ft-lb/in² | Average value: 38.3 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 45.0 kJ/m² | 7.14 - 21.4 ft-lb/in² | Average value: 27.0 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 45.0 kJ/m² @Temperature -40.0 - -30.0 °C |
11.9 - 21.4 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 34.4 kJ/m² Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 45.0 kJ/m² | 11.9 - 21.4 ft-lb/in² | Average value: 33.3 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |