Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.30 J/cm² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Charpy Impact Unnotched | 8.30 J/cm² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Charpy Impact Unnotched | 8.30 J/cm² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1017GH33 BK701 PA6-GF33 33% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact Unnotched | 8.30 J/cm² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.30 J/cm² @Temperature 23.0 °C |
39.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com.. |