Polymer Property : Tensile Stress = 4350 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 30.0 MPa
4350 psi
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Tensile Stress 30.0 MPa
4350 psi
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified
Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG
Tensile Stress 30.0 MPa
4350 psi
ISO R527
Iran Petrochemical (PCC) EP-N31MA Polypropylene
EP-N31MA is a high ultra fluidity heterophasic copolymer for thin walled injection molding the products offers a good stiffness impact balance. Applications: packaging, house ware and garden furnitu..
Tensile Stress 30.0 MPa
4350 psi
ISO R527
Iran Petrochemical (PCC) V 30 S Polypropylene
V 30 S is a high fluidity PP for the protection of staple fibers with improved thermo bonding ability for no woven fabrics.Application: the typical application of this grade are cover stock for diap..
Tensile Stress 30.0 MPa
4350 psi
at Break; ISO 527
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene
I3 is a high density polyethylene with 1-Butene as co monomer. It has low warpage, good flowability, high density, hardness and stiffness, good impact strength, and good stress cracking resistance...
Tensile Stress 30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® TSZ 3 PA666
Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug..
Tensile Stress 30.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
4350 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® DYM1300 BK320 TPC-ET  (Unverified Data**)
Hytrel® DYM1300 is a high performance thermoplastic elastomer with high modulus, suited for air bag door applications.Information provided by DuPont Performance Polymers
Tensile Stress 30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® FN727 NC010A Nylon 6  (Unverified Data**)
Toughened Polyamide 6Information provided by DuPont Performance Polymers
Tensile Stress 30.0 MPa

@Strain 10.0 %,
Temperature 23.0 °C
4350 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8539 BK316 TPC-ET  (Unverified Data**)
Hytrel® HTR8539 is a 72 Shore D, plasticiser free, high performance resin for extrusion. It has high viscosity.Information provided by DuPont Performance Polymers