Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | ASTM D638 |
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | ASTM D4894 |
3M Dyneon™ TFM™ 1600 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Dyneon TFM 1600 PTFE is a free-flowing powder for compression molding, isostatic molding, automatic molding, and ram extrusion. Dyneon™ TFM™ 1600 PTFE is a second-generatio.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
Ineos CP53-30 Polyethylene Copolymer CP53-30 is a high density polyethylene copolymer developed for corrugated piping applications. This product is recommended for use in applications that are required to meet AASHTO specifications M 2.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | ASTM-D638 |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | at max load; ASTM D638 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | at max load; ASTM D638 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | at max load; ASTM D638 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | at max load; ASTM D638 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | at max load; ASTM D638 |
A. Schulman PP 1667-01 Polypropylene Natural Homopolymer Polypropylene DescriptionPolypropylene PP 1667-01 is an easy flowing natural homopolymer polypropylene. It is for injection molding large parts with thin sections requiring good stiffness, heat resistance, and c.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 10 s set time |
Elmer's Products Aron Alpha® 221 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 3 s set time |
Elmer's Products Aron Alpha® 221F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 3 s set time |
Elmer's Products Aron Alpha® 231F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 15 s set time |
Elmer's Products Aron Alpha® 241F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 15 s set time |
Elmer's Products Aron Alpha® 282F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. rigid PVC; 5 s set time |
Elmer's Products Aron Alpha® 801 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Low gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. .. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | Compression molded parts prepared according to ASTM D 1928 Procedure C.; ASTM D638 |
Dow DGDA-2475 NT High Density Polyethylene Resin DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in corrugated pipe applications. It has been specifically designed for extrusion of corrugated pipes with the.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 15 s set time |
Elmer's Products Aron Alpha® 241E Cyanoacrylate Adhesive (Industrial Krazy Glue™) For clean, fast applications. Best for high speed automated assembly.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous subs.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 15 s set time |
Elmer's Products Aron Alpha® 252E Cyanoacrylate Adhesive (Industrial Krazy Glue™) For clean, fast applications. Best for high speed automated assembly.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous sub.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | vs. steel; 10 s set time |
Elmer's Products Aron Alpha® 252F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TFM™ 1600 PTFE Meets ASTM D4894 Type III, Grade 2 resinMolding and ram extrusion powder with very good free flowing propertiesGood metering propertiesGood mold filling behaviorImproved particle coalescenceDenser p.. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® GPA100 ABS High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength at Break | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |