Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elmer's Products Aron Alpha® 231F Cyanoacrylate Adhesive (Industrial Krazy Glue™)

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Elmer's Products, Inc.
Trade Name Aron Alpha®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elmer's Products Aron Alpha® 231F Cyanoacrylate Adhesive (Industrial Krazy Glue™).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on a variety of materials.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous substrates. Military Spec MIL-A-46050C Type 2. Military Spec MIL-A-46050C Class 1. A primer is required for hard-to-bond materials such as polyethylene, polypropylene, acetal, PET, nylon, soft PVC, silicone rubber, and glass.General information about the Aron Alpha® product line: Cyanoacrylates are single component instant adhesives that bond a wide variety of surfaces with a strong, durable bond. They offer ease of application, a wide range of performance parameters, and reliable solvent-free bonding.Toagosei Co., Ltd. produces cyanoacrylates in Japan, marketed as Aron Alpha® in Japan, Cyanolit® in Europe, and Krazy Glue® in the US. Elmer's Products markets Krazy Glue® to the retail trade and Aron Alpha® to the industrial trade in North America. Information provided by Elmer's Products, Inc.
Physical Properties Metric English Comments
Viscosity 30 cP
30 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.48 MPa
360 psi
vs. neoprene chloroprene (CR); 1 s set time
19.3 MPa
2800 psi
vs. aluminum; 5 s set time
31.7 MPa
4600 psi
vs. steel; 3 s set time
34.5 MPa
5000 psi
vs. rigid PVC; 1 s set time
34.5 MPa
5000 psi
vs. polycarbonate; 3 s set time
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Estimated; Manufacturer specifies clear but does not quantify.
Processing Properties Metric English Comments
Processing Temperature 20.0 °C
68.0 °F
typically used at ambient temperature
Descriptive Properties Value Comments
Color Clear
Users viewing this material also viewed the following: