Material Notes:
Meets ASTM D4894 Type III, Grade 2 resinMolding and ram extrusion powder with very good free flowing propertiesGood metering propertiesGood mold filling behaviorImproved particle coalescenceDenser polymer structureLower permeabilitySubstantially lower deformation under loadImproved weldabilityGood electrical and mechanical propertiesIncreased modulus of elasticityInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.16 g/cc
2.16 g/cc
@ 23°C, Sintering Molding; ASTM D4894-98a
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894-98a
Particle Size 450 µm
450 µm
average; ASTM D4894-98a
Deformation 4.0 %
4.0 %
2175 psi - permanent, 23°C, Sintering Molding; ASTM D621
8.0 %
8.0 %
2175 psi - 24 hrs, 23°C, Sintering Molding; ASTM D621
9.0 %
9.0 %
2175 psi - 100 hrs, 23°C, Sintering Molding; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.7 MPa
4600 psi
Sintered Molding; ASTM D4894-98a
Elongation at Break 450 %
450 %
Sintered Molding; ASTM D4894-98a
Tensile Modulus 0.6498 GPa
94.25 ksi
Sintered Molding; ASTM D638
Thermal Properties Metric English Comments
Melting Point 317 - 337 °C
603 - 639 °F
second; ASTM D4894-98a
332 - 352 °C
630 - 666 °F
initial; ASTM D4894-98a
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-330 °F
Flammability, UL94 V-0
V-0
Shrinkage 3.50 %

@Temperature 23.0 °C
3.50 %

@Temperature 73.4 °F
Sintering Moldings; ASTM D4894-98a
Electrical Properties Metric English Comments
Dielectric Strength 102.4 kV/mm
2601 kV/in
ASTM D149-95a