Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.6 MPa | 4000 psi | TM R050-36 |
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2 in/min; ASTM D638 |
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black Applications: BracketsAir ductsConsolesWire troughInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D4894 |
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **) Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D4894 |
3M Dyneon™ 1641 PTFE Powder
(discontinued **) Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
LyondellBasell Alathon® L5332CP High Density Polyethylene, Blow Molding Grade ALATHON L5332CP is bimodal molecular weight distribution, fractional melt index HDPE resin that exhibits an exceptional balance of environmental stress crack resistance and stiffness. Typical applic.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tensile Strength at Break | 27.6 - 38.6 MPa | 4000 - 5600 psi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tensile Strength at Break | 27.6 - 31.0 MPa | 4000 - 4500 psi | |
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1377A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | >= 27.6 MPa | >= 4000 psi | |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Eastman Tenite 285A2R30020 Cellulose Acetate Butyrate, Natural, Trsp Applications:Tool handlesToys/sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clar.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Tensile Strength at Break | >= 27.58 MPa | >= 4000 psi | Sintered Molding; ASTM D4894-98a |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
Chesterton MRS 10 Metal Rebuilding System Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10.. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength at Break | 27.6 MPa | 4000 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |