Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 27.5 MPa @Thickness 2.00 mm |
3990 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 27.5 MPa | 3990 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 556 Flame Retardant Polystyrene Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect.. |
|||
Tensile Strength at Break | 27.5 MPa | 3990 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 566 Flame Retardant Polystyrene Characteristics Good flow and toughness Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Available in any color Processing Extrusion MoldingApplications Large size T.V. Cabinets El.. |
|||
Tensile Strength at Break | 27.5 MPa | 3990 psi | ACMA Test #4 / DIN EN 843-1 |
CeramTec 701 Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Tensile Strength at Break | 27.5 MPa @Temperature 160 - 175 °C, Time 1.80e+7 sec |
3990 psi @Temperature 320 - 347 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Conditioned, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Tensile Strength at Break | 27.5 MPa @Temperature 130 - 150 °C, Time 7.20e+7 sec |
3990 psi @Temperature 266 - 302 °F, Time 20000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Conditioned, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |