Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 197 MPa | 28600 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 1200 A 33 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | ASTM D638 |
LNP Lubricomp® UFL-4036 HS Polyphthalamide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | ASTM D638 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | d.a.m.; ISO 527-1, -2; 5 mm/min |
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EC002XXQ PEI LNP* THERMOCOMP* EC002XXQ is a compound based on Polyetherimide containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF00AS PA 66 LNP THERMOCOMP* RF00AS is a compound based on Nylon 66 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66 LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation .. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Tensile Strength at Break | 197 MPa | 28600 psi | ASTM D638 |
LNP Lubricomp® BGU- Polyphthalamide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: Heat Stabilized, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP gr.. |