Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 72.4 MPa | 10500 psi | 2 in/min; ASTM D638 |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | 2 in/min; ASTM D638 |
RheTech Products GC20P200-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsBoat handlesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
M. Holland Company PC406UR Polycarbonate High impact resistanceGood mold releaseGood UV resistanceHigh viscosityApplications: AppliancesProtective coveringsDecorative displaysHousings |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D638 |
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D882 |
Westlake Plastics PES film Made from ULTRASON® E Polyethersulfone Resin High heat deflection and continuous use temperature. Exceptional tensile and flexural strength. High dielectric strength. Exceptional mechanical properties. Dimensionally stable at varying tempera.. |
|||
Tensile Strength at Break | 72.4 MPa | 10500 psi | ASTM D3574 |
3M 435 Vibration Damping Tape 3M™ Vibration Damping Tapes are low temperature 3M™ Viscoelastic Damping Polymers Tape 830 coated on the dead soft aluminum foil constraining layer. They have pressure sensitive properties and are.. |
|||
Tensile Strength at Break | 72.3 MPa | 10500 psi | ASTM D3759 |
3M 853 Polyester Tape 3M™ Polyester Tape 853 is comprised of strong, thin polyester backing with high shear, solvent resistant acrylic adhesive. These qualities make this tape ideal for applications where solvent exposu.. |