Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.76 MPa | 400 psi | TM R050-36 |
Resinlab® EP1121 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Clear is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |
|||
Tensile Strength at Break | 2.76 MPa @Temperature 23.0 °C |
400 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE) Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics |
|||
Tensile Strength at Break | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1240 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Tensile Strength at Break | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1798 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1586 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1586UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP-1662-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2287N Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP 1736R Thermoplastic Elastomer Notes: Soft Material; Overmold onto PP handlesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tensile Strength at Break | 2.76 - 3.45 MPa | 400 - 500 psi | |
Master Bond MasterSil 153Med Silicone Paste for Medical Applications Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it.. |
|||
Tensile Strength at Break | 2.76 - 3.45 MPa | 400 - 500 psi | |
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of .. |
|||
Tensile Strength at Break | 2.76 - 3.45 MPa | 400 - 500 psi | |
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D638 - ISO 527-2 |
DuPont Keldax® 6868 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D638 - ISO 527-2 |
DuPont Keldax® 6798 Filled Thermoplastic Ethylene Polymer A low fog filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailabil.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D638 |
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | JRF- 72 hrs @ 60°C, and 72 hrs @ 49°C, and 7 days @ 121°C |
3M AC-240 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | Standard Cure |
3M AC-350 Class A-1 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | Standard Cure |
3M AC-350 Class A-1/2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | Standard Cure |
3M AC-350 Class A-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class A are fast-cure, intermediate density two-component, manganese dioxide cure, brushable, polysulfide fuel tank and fuselage sealants. 3M AC-350 Class A Sealants have.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | ASTM D412 |
Teknor Apex Monprene® MP-2730 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | TM R050-36 |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | JRF- 72 hrs @ 60°C, and 72 hrs @ 49°C, and 7 days @ 121°C |
3M AC-240 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-240 Class B is a two-part, polysulfide-based, long application life, quick cure product for use as a sealant for integral fuel tanks and fuselages. This tow-component, mangan.. |
|||
Tensile Strength at Break | 2.76 MPa | 400 psi | TM R050-36 |
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. I.. |