Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.85 J/cm @Temperature 23.0 °C |
9.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS (Asia Pacific) LNP* Lubricomp* OCP36 is a compound based on Polyphenylene Sulfide resin containing Carbon Fiber, Lubricants, Bearing Grade. Added features of this material include: Internally Lubricated, Electric.. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Bearing Grade, Electrically Conductive, Wear R.. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.85 J/cm @Temperature 23.0 °C |
9.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX99873C PC LNP STAT-KON* DX99872C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 4.85 J/cm | 9.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Izod Impact, Unnotched | 4.85 J/cm @Temperature 23.0 °C |
9.09 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific) LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp.. |