Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D-4812 |
PlastiComp Velocity® LCF40-PA66 High Flow Nylon 66, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC LNP STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Clean Compounding System. Easy Molding, Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 6.92 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66 LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Ensinger TECASON™ P Polyphenylsulfone (PPSU) TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties. |
|||
Izod Impact, Unnotched | 6.94 - 11.7 J/cm | 13.0 - 22.0 ft-lb/in | Average value: 10.5 J/cm Grade Count:8 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36E PC LNP LUBRICOMP* DFL36E is a compound based on Polycarbonate resin containing 30% Glass Fiber, 155 PTFE. Added features of this material include: Easy Molding, Internally Lubricated. |