Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 240 Rigid PVC, Extrusion Electric channels |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 241 Rigid PVC, Extrusion Various profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 325/2 Rigid PVC, Extrusion Building profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 337 Rigid PVC, Extrusion Cheap profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 612 Rigid PVC, Extrusion Spiral pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 620 Rigid PVC, Extrusion Spiral pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 52 Rigid PVC, Injection Molding Fittings for building trade |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 54 Rigid PVC, Injection Molding Fittings for building trade - high fluidity |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 55 Rigid PVC, Injection Molding Fittings for building trade - high fluidity |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 0758 Rigid PVC, Extrusion Lead Free Electric corrugated pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 316 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 320 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 325 Rigid PVC, Extrusion Lead Free Verticle curtains |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free Profiles anti mould |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free Profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 435 Rigid PVC, Extrusion Lead Free Electrical channels |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RL 708 Rigid PVC, Extrusion Corrugated electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RL 710 Rigid PVC, Extrusion Corrugated electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RST 171 Rigid PVC, Extrusion Lead Free Various transparent profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 220 Rigid PVC, Extrusion Rolling shutters |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 220/R Rigid PVC, Extrusion Shiny rolling shutters |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 116 Rigid PVC, Extrusion Small tubes for shoes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds R 244 Rigid PVC, Extrusion Shutters high modulus low curving |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 225/R Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 235 Rigid PVC, Extrusion Electric channels and profiles |
|||
Izod Impact, Unnotched | 0.400 - 0.800 J/cm @Temperature 23.0 °C |
0.749 - 1.50 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 236 Rigid PVC, Extrusion Electric channels |