Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.80 J/cm | 5.25 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu.. |
|||
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 206/C Rigid PVC, Antishock Extrusion Medium antishock profiles |
|||
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 612 Rigid PVC, Antishock Extrusion Medium antishock profiles |
|||
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 311 Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Izod Impact, Unnotched | 2.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
5.25 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Izod Impact, Unnotched | 2.80 J/cm | 5.25 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Unnotched | 2.80 J/cm @Temperature -30.0 °C |
5.25 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched | 2.80 J/cm | 5.25 ft-lb/in | ASTM D256 |
Styrolution NAS® 90 High Performance Styrenic NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla.. |
|||
Izod Impact, Unnotched | 2.80 J/cm | 5.25 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Unnotched | 2.80 - 7.45 J/cm @Temperature -30.0 - -30.0 °C |
5.25 - 14.0 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 4.67 J/cm Grade Count:8 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |