Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-G30 ABS, 30% Glass Reinforced Acrylonitrile Butadiene Styrene, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Izod Impact, Unnotched | 2.67 - 7.01 J/cm | 5.00 - 13.1 ft-lb/in | Average value: 5.28 J/cm Grade Count:21 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Thickness 3.18 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® ECL-4036 Polyetherimide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp OX95338 PPS LNP* Lubricomp* OX95338 is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.Thi.. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp OX95338 PPS (Asia Pacific) LNP* Lubricomp* OX95338 is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.Thi.. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-40TC-8100 40% Talc Reinforced, Heat Stabilized Information provided by Asahi Thermofil |