Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Izod Impact, Unnotched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 2.61 J/cm @Temperature 23.0 °C |
4.89 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Izod Impact, Unnotched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Izod Impact, Unnotched | 2.61 J/cm | 4.89 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |