Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
PlastiComp Complet® LCF30-PA66 30% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS (Asia Pacific) LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D4812 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFL16 PA 66 (Asia Pacific) LNP LUBRICOMP* RFL16 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 10.68 J/cm @Temperature 23.0 °C |
20.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by .. |
|||
Izod Impact, Unnotched | 10.68 J/cm @Temperature 23.0 °C |
20.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp RFL16S PA 66 (Asia Pacific) LNP* Lubricomp* RFL16S is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.This data was supplied by .. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX03571 PC LNP* STAT-KON* DX03571 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX05475 PC LNP* THERMOCOMP* DX05474 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Asia Pacific) LNP* Thermocomp* PF006U is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: UV Stabilized. |
|||
Izod Impact, Unnotched | 10.68 J/cm @Temperature 23.0 °C |
20.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 (Asia Pacific) LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCL36 PA 66 LNP* LUBRICOMP* RCL36 is a compound based on Nylon 66 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wesr Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 10.68 J/cm | 20.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 10.68 J/cm @Temperature 23.0 °C |
20.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermotuf PC006I PA 6 LNP* Thermotuf* PC006I is a compound based on Nylon 6 resin containing Carbon Fiber, Impact Modifier. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the.. |