Polymer Property : Izod Impact, Unnotched = 0.534 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA66BK Nylon 66
Information provided by Niche Polymer
Izod Impact, Unnotched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 0.534 - 2.94 J/cm
1.00 - 5.51 ft-lb/in
Average value: 1.67 J/cm Grade Count:19
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Unnotched 0.534 - 5340 J/cm
1.00 - 10000 ft-lb/in
Average value: 9.81 J/cm Grade Count:19
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
Izod Impact, Unnotched 0.534 - 13.0 J/cm
1.00 - 24.4 ft-lb/in
Average value: 5.23 J/cm Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS); Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched 0.534 J/cm - NB
1.00 ft-lb/in - NB
Average value: 9.53 J/cm Grade Count:9
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Unnotched 0.534 J/cm

@Temperature -40.0 °C
1.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech SolarKote® /ABS Weatherable Sheet
Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech.
Izod Impact, Unnotched 0.534 J/cm

@Temperature -40.0 °C
1.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Spartech SP-9070 ABS/PVC Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
Izod Impact, Unnotched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM)
TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop..
Copyright © lookpolymers.com All Rights Reserved