Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 42.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.40 - 9.00 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.55 J/cm² Grade Count:8
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 1.50 - 9.00 J/cm²
7.14 - 42.8 ft-lb/in²
Average value: 4.07 J/cm² Grade Count:9
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 4.00 - 9.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.47 J/cm² Grade Count:10
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Charpy Impact Unnotched 2.00 - 9.00 J/cm²

@Temperature -30.0 - 30.0 °C
9.52 - 42.8 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 4.20 J/cm² Grade Count:26
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact Unnotched 2.50 - 9.00 J/cm²
11.9 - 42.8 ft-lb/in²
Average value: 5.50 J/cm² Grade Count:3
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Charpy Impact Unnotched 4.00 - 9.00 J/cm²

@Temperature -30.0 - -20.0 °C
19.0 - 42.8 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 7.25 J/cm² Grade Count:6
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Charpy Impact Unnotched 2.40 - 9.00 J/cm²

@Temperature -40.0 - -20.0 °C
11.4 - 42.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.51 J/cm² Grade Count:28
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Charpy Impact Unnotched 2.20 - 9.00 J/cm²

@Temperature -40.0 - -30.0 °C
10.5 - 42.8 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 4.59 J/cm² Grade Count:16
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Charpy Impact Unnotched 2.30 - 9.00 J/cm²
10.9 - 42.8 ft-lb/in²
Average value: 5.30 J/cm² Grade Count:10
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Charpy Impact Unnotched 2.00 - 9.00 J/cm²
9.52 - 42.8 ft-lb/in²
Average value: 4.88 J/cm² Grade Count:24
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 3.80 - 9.00 J/cm²
18.1 - 42.8 ft-lb/in²
Average value: 6.26 J/cm² Grade Count:30
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact Unnotched 3.20 - 9.00 J/cm²

@Temperature -20.0 - 0.000 °C
15.2 - 42.8 ft-lb/in²

@Temperature -4.00 - 32.0 °F
Average value: 6.10 J/cm² Grade Count:2
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 4.50 - 9.00 J/cm²

@Temperature -30.0 - -20.0 °C
21.4 - 42.8 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 6.50 J/cm² Grade Count:7
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..
Copyright © lookpolymers.com All Rights Reserved