Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.700 - 1.00 J/cm² @Temperature 23.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact Unnotched | 0.700 - 1.00 J/cm² @Temperature 23.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact Unnotched | 0.600 - 1.00 J/cm² | 2.86 - 4.76 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact Unnotched | 1.00 - 1.00 J/cm² @Temperature -20.0 - -20.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.00 J/cm² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 802 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² @Temperature 23.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group RALUPOL® 8601 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² @Temperature 23.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eU |
Raschig Group RALUPOL® 8602 UP Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng.. |
|||
Charpy Impact Unnotched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact Unnotched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | ISO 179 |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact Unnotched | 0.850 - 1.00 J/cm² | 4.05 - 4.76 ft-lb/in² | ISO 179 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Charpy Impact Unnotched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | ISO 179 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Charpy Impact Unnotched | 0.500 - 1.00 J/cm² | 2.38 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Charpy Impact Unnotched | 0.700 - 1.00 J/cm² | 3.33 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |