Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.00 - 4.50 J/cm²
14.3 - 21.4 ft-lb/in²
Average value: 3.90 J/cm² Grade Count:10
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Charpy Impact Unnotched 3.00 - 4.50 J/cm²
14.3 - 21.4 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:3
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 1.40 - 4.50 J/cm²
6.66 - 21.4 ft-lb/in²
Average value: 3.24 J/cm² Grade Count:7
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 2.50 - 4.50 J/cm²
11.9 - 21.4 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Charpy Impact Unnotched 1.00 - 4.50 J/cm²

@Temperature -40.0 - -20.0 °C
4.76 - 21.4 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.58 J/cm² Grade Count:12
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 2.00 - 4.50 J/cm²
9.52 - 21.4 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound
UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit..
Charpy Impact Unnotched 2.50 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
11.9 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.75 J/cm² Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Charpy Impact Unnotched 2.00 - 4.50 J/cm²
9.52 - 21.4 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:5
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 4.50 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Charpy Impact Unnotched 4.50 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
21.4 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.50 J/cm² Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Charpy Impact Unnotched 1.50 - 4.50 J/cm²
7.14 - 21.4 ft-lb/in²
Average value: 3.37 J/cm² Grade Count:7
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Charpy Impact Unnotched 3.00 - 4.50 J/cm²
14.3 - 21.4 ft-lb/in²
Average value: 3.50 J/cm² Grade Count:3
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Charpy Impact Unnotched 4.00 - 4.50 J/cm²

@Temperature -30.0 - -20.0 °C
19.0 - 21.4 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 4.25 J/cm² Grade Count:2
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Charpy Impact Unnotched 2.00 - 4.50 J/cm²
9.52 - 21.4 ft-lb/in²
Average value: 3.26 J/cm² Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
Charpy Impact Unnotched 3.00 - 4.50 J/cm²

@Temperature -30.0 - -30.0 °C
14.3 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.75 J/cm² Grade Count:4
Overview of materials for Polytrimethylene Terephthalate (PTT)
This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val..
Copyright © lookpolymers.com All Rights Reserved