Polymer Property : Charpy Impact Unnotched = 4759 ft-lb/in² - NB Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 999.9 J/cm² - NB

@Temperature -60.0 - -30.0 °C
4759 ft-lb/in² - NB

@Temperature -76.0 - -22.0 °F
Grade Count:14
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact Unnotched 999.9 J/cm² - NB

@Temperature -60.0 - -30.0 °C
4759 ft-lb/in² - NB

@Temperature -76.0 - -22.0 °F
Grade Count:10
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -60.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -76.0 - -22.0 °F
Grade Count:6
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -60.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -76.0 - -22.0 °F
Grade Count:20
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Grade Count:2
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -20.0 - -20.0 °C
4759 - 4759 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Grade Count:1
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Grade Count:7
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Charpy Impact Unnotched 999.9 - 999.9 J/cm²

@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Grade Count:2
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Charpy Impact Unnotched 999.9 J/cm² - NB

@Temperature -30.0 - -30.0 °C
4759 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Grade Count:40
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..