Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK4122H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,078-06-04-23 UL94 V-2, halogen and antimony free, medium impact polystyrene. This grade features enhanced thermal stabi.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² - NB | 40.5 ft-lb/in² - NB | Average value: 9.25 J/cm² Grade Count:25 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² - NB @Temperature -30.0 - -30.0 °C |
40.5 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Average value: 10.1 J/cm² Grade Count:23 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | Conditioned; ISO 179/1eU |
Solvay Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant This Red Phosphorous and Halogen free flame retardant grade, combines excellent all-round mechanical properties with outstanding flame retardancy (UL 5VA at 1.6mm) and electrical performance. This p.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 20 HWCP 20% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.5 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | |
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Charpy Impact Unnotched | 8.50 J/cm² | 40.5 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® MN301-G30 Nylon 66 Resin 30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |