Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.30 - 8.00 J/cm² | 10.9 - 38.1 ft-lb/in² | Average value: 4.42 J/cm² Grade Count:44 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 1.40 - 8.00 J/cm² @Temperature -40.0 - 30.0 °C |
6.66 - 38.1 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 5.20 J/cm² Grade Count:84 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Charpy Impact Unnotched | 1.30 - 8.00 J/cm² @Temperature -40.0 - -30.0 °C |
6.19 - 38.1 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.15 J/cm² Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.00 - 8.00 J/cm² @Temperature -40.0 - -20.0 °C |
9.52 - 38.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.27 J/cm² Grade Count:65 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Charpy Impact Unnotched | 2.00 - 8.00 J/cm² @Temperature -30.0 - -20.0 °C |
9.52 - 38.1 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 5.21 J/cm² Grade Count:26 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact Unnotched | 1.10 - 8.00 J/cm² @Temperature -40.0 - -20.0 °C |
5.24 - 38.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.34 J/cm² Grade Count:9 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Charpy Impact Unnotched | 3.50 - 8.00 J/cm² | 16.7 - 38.1 ft-lb/in² | Average value: 5.17 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Charpy Impact Unnotched | 3.00 - 8.00 J/cm² @Temperature -40.0 - -20.0 °C |
14.3 - 38.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.67 J/cm² Grade Count:3 |
Overview of materials for Nylon 66, 40% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in.. |
|||
Charpy Impact Unnotched | 3.20 - 8.00 J/cm² @Temperature -30.0 - -30.0 °C |
15.2 - 38.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.07 J/cm² Grade Count:9 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 5.20 - 8.00 J/cm² @Temperature -40.0 - -20.0 °C |
24.7 - 38.1 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 6.57 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact Unnotched | 2.10 - 8.00 J/cm² | 9.99 - 38.1 ft-lb/in² | Average value: 5.82 J/cm² Grade Count:18 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 4.00 - 8.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 38.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.71 J/cm² Grade Count:7 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 3.50 - 8.00 J/cm² | 16.7 - 38.1 ft-lb/in² | Average value: 5.88 J/cm² Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide + Glass/PTFE". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 1.50 - 8.00 J/cm² | 7.14 - 38.1 ft-lb/in² | Average value: 5.53 J/cm² Grade Count:33 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Charpy Impact Unnotched | 2.00 - 8.00 J/cm² | 9.52 - 38.1 ft-lb/in² | Average value: 6.12 J/cm² Grade Count:16 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |
|||
Charpy Impact Unnotched | 4.50 - 8.00 J/cm² | 21.4 - 38.1 ft-lb/in² | Average value: 6.56 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |