Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.50 - 3.50 J/cm² @Temperature -40.0 - -20.0 °C |
16.7 - 16.7 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 3.50 J/cm² Grade Count:1 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 2.50 - 3.50 J/cm² | 11.9 - 16.7 ft-lb/in² | Average value: 3.08 J/cm² Grade Count:6 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact Unnotched | 3.50 - 3.50 J/cm² @Temperature -30.0 - -30.0 °C |
16.7 - 16.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.50 J/cm² Grade Count:1 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact Unnotched | 3.50 - 3.50 J/cm² @Temperature -30.0 - -30.0 °C |
16.7 - 16.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.50 J/cm² Grade Count:1 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact Unnotched | 1.90 - 3.50 J/cm² | 9.04 - 16.7 ft-lb/in² | Average value: 2.54 J/cm² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact Unnotched | 2.60 - 3.50 J/cm² | 12.4 - 16.7 ft-lb/in² | Average value: 3.03 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 2.20 - 3.50 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 16.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 2.85 J/cm² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 3.00 - 3.50 J/cm² | 14.3 - 16.7 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |