Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Charpy Impact Unnotched | 0.700 - 0.900 J/cm² | 3.33 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Charpy Impact Unnotched | 0.700 - 0.900 J/cm² | 3.33 - 4.28 ft-lb/in² | Injection and Compression; ISO 179/1eU |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Charpy Impact Unnotched | 0.700 - 0.900 J/cm² | 3.33 - 4.28 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Charpy Impact Unnotched | 0.600 - 0.900 J/cm² | 2.86 - 4.28 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Charpy Impact Unnotched | 0.700 - 0.900 J/cm² | 3.33 - 4.28 ft-lb/in² | ISO 179 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Charpy Impact Unnotched | 0.750 - 0.900 J/cm² | 3.57 - 4.28 ft-lb/in² | ISO 179 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |
|||
Charpy Impact Unnotched | 0.200 - 0.900 J/cm² | 0.952 - 4.28 ft-lb/in² | Average value: 0.590 J/cm² Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |