Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 999.9 J/cm² - NB @Temperature -60.0 - -30.0 °C |
4759 ft-lb/in² - NB @Temperature -76.0 - -22.0 °F |
Grade Count:14 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact Unnotched | 999.9 J/cm² - NB @Temperature -60.0 - -30.0 °C |
4759 ft-lb/in² - NB @Temperature -76.0 - -22.0 °F |
Grade Count:10 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -60.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -76.0 - -22.0 °F |
Grade Count:6 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -60.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -76.0 - -22.0 °F |
Grade Count:20 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Grade Count:2 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -20.0 - -20.0 °C |
4759 - 4759 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Grade Count:1 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Grade Count:7 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact Unnotched | 999.9 - 999.9 J/cm² @Temperature -30.0 - -30.0 °C |
4759 - 4759 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Grade Count:2 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact Unnotched | 999.9 J/cm² - NB @Temperature -30.0 - -30.0 °C |
4759 ft-lb/in² - NB @Temperature -22.0 - -22.0 °F |
Grade Count:40 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |