Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 20.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
dry; ISO 179-1/1eU
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Charpy Impact Unnotched >= 20.0 J/cm²
>= 95.2 ft-lb/in²
ISO 179
Murtfeldt Murytal® H Acetal Homopolymer
In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it..
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
ISO 179/1eU
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin
Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov..
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
49 HRC
International Mold Steel DHA-World Die Cast & Forging Steel
DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo..
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
BASF Novolen® 3240 NC Polypropylene
Grade containing nucleating agent for transparent injection molded parts.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
ISO 179
BASF Ultraform N 2310P Q600 POM
Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert..
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
ISO 179
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
BASF Novolen® 2240 P Polypropylene
Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 20.0 J/cm²
95.2 ft-lb/in²
BASF Novolen® 3248 RC Polypropylene
Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF.
Copyright © lookpolymers.com All Rights Reserved