Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO Data, Low Temp |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV35 Nylon 6.6 for injection molding, 35% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.00 - 6.50 J/cm² | 9.52 - 30.9 ft-lb/in² | Average value: 4.05 J/cm² Grade Count:12 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.00 J/cm² - NB | 9.52 ft-lb/in² - NB | Average value: 2.63 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Charpy Impact Unnotched | 2.00 - 5.00 J/cm² @Temperature -30.0 - -20.0 °C |
9.52 - 23.8 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.00 J/cm² Grade Count:11 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1/AR/5/NT Polyamide 66, with aramid reinforcement Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Isotropic shrinkage characteristics.Control disks, cams, s.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® G Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® GS-H/2 Polyamide 66, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Isotropic shrinkage characteristics.Control disks, cams, sliding ele.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179 |
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² @Temperature 23.0 °C |
9.52 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | |
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | |
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo.. |
|||
Charpy Impact Unnotched | 2.00 J/cm² | 9.52 ft-lb/in² | |
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |