Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT PA6 Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in natural as well as full RAL color scale.Information Prov.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT B 27 A PA66 PA66 for compounding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, h.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 15 002/1M PA66 reinforced with glass fiber PA66 for injection molding, reinforced with 15 % glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools,.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC GK8020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS15020 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² @Temperature 23.0 °C |
1.19 - 1.67 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/1eU |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² @Temperature 23.0 °C |
1.19 - 1.67 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group RALUPOL® 4385 UP Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH 30030DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² @Temperature 23.0 °C |
1.19 - 1.67 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179 1eA |
Raschig Group SURAPLAST 54 UPA Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-4120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-4120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form as well.INNOPOL® CS 2-4120 is developed for p.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
|
LATI Lapex A PES Polyether Sulfone (PES). Unfilled. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BH980MO Polypropylene Copolymer BH980MO is a heterophasic copolymer. This grade provides very high stiffness, high gloss and low stress whitening. and is designed for high-speed injection molding and contains nucleating and antist.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 GB 20 PA6 reinforced with 20% glass beads Features: Nearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical proper.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T8020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS8030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultramid® B3UGM210 GR 22866 10/50% Glass/Mineral Filled PA6 FR (Dry) Description: Halogen- and phosphorus-free injection-molding grade with very high rigidity, low smoke density and outstanding electrical properties.Information provided by BASF |