Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 32 C PA66 PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 32 C PA66 PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 51 C 40 PP reinforced with 40% mineral filler Features: Modified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified chalk. Increased strength, rigidity and thermal application up to 100.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitabl.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 20 LS PA6, 20% glass beads, light stability FeaturesStabilized against UV radiation. External use. PA 6 for injection moulding, reinforced with 20% glass beads offers high grade surface brightness, low rolling resistance force. Application: e.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, .. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 GB 20 LS PA66, 20% glass beads, light stability FeaturesPA 66 for injection moulding, chemically reinforced with 20 % glass beads, light stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and elect.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® E BT N PET Basic type PET for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fast.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 56 T FRD 1 PP, flame retardant FeaturesModified homopolymer PP for injection moulding with decreased flammability. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil forms, guides, co.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packag.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® AG9H MI/40 PP Homopolymer, 40% Mica Reinforced, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Mica filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PKN4766 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4766 is a translucent PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulat.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daploy™ WB140HMS Polypropylene Daploy™ WB140HMS is a structurally isomeric modified propylene homopolymer. Applications: door liners, parcel shelves, microwaveable food packaging, cushioning and protective packaging, lightweigh.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 GF 15 Polypropylene Homopolymer, 15% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 15% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers |