Polymer Property : Charpy Impact, Notched = 0.294 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.294 J/cm²

@Temperature -30.0 °C
1.40 ft-lb/in²

@Temperature -22.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s..
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CMU 201 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior covered applications such as retainers in which a good stiffness toughness balance is required.Availa..
Charpy Impact, Notched 0.294 J/cm²

@Temperature 0.000 °C
1.40 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CMW 203 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by high flow and designed for automotive interior applications such as door panel linings and other low pressure back mo..
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNK 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection or extrusion automotive applications with low melt and excellent low temperature impact. Availability: Africa &..
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
ExxonMobil PPU0009F Polypropylene Impact Copolymer
Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobi..