Material Notes:
Product Description: A specialty thermoplastic polyolefin resin characterized by high flow and designed for automotive interior applications such as door panel linings and other low pressure back molding applications.Availability: Africa & Middle East, Asia Pacific, Europe, South America and North America Features: Good Dimensional Stability Good Impact ResistanceGood Mold ReleaseHigh FlowUses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior Trim Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 40 g/10 min

@Load 2.16 kg,
Temperature 230 °C
40 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 21.0 MPa
3050 psi
ISO 527-2/50
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2/50
Elongation at Break 7.0 %
7.0 %
ISO 527-2/50
Elongation at Yield 2.6 %
2.6 %
ISO 527-2/50
Tensile Modulus 2.50 GPa
363 ksi
Secant; ISO 527-2
Charpy Impact, Notched 0.210 J/cm²

@Temperature -20.0 °C
1.00 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
0.294 J/cm²

@Temperature 0.000 °C
1.40 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
0.504 J/cm²

@Temperature 22.8 °C
2.40 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
241 °F
ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F
ISO 75-2/A