Mechanical Properties Metric English Comments
Izod Impact, Notched 1.00 - 1.10 J/cm
1.87 - 2.06 ft-lb/in
Average value: 1.03 J/cm Grade Count:3
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Izod Impact, Notched 0.320 - 1.10 J/cm
0.600 - 2.06 ft-lb/in
Average value: 0.618 J/cm Grade Count:4
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 1.10 - 1.10 J/cm

@Temperature -40.0 - -40.0 °C
2.06 - 2.06 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.10 J/cm Grade Count:1
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Izod Impact, Notched 0.700 - 1.10 J/cm

@Temperature -40.0 - 0.000 °C
1.31 - 2.06 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.945 J/cm Grade Count:2
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Notched 0.700 - 1.10 J/cm

@Thickness 3.20 - 3.20 mm
1.31 - 2.06 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 0.945 J/cm Grade Count:2
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Notched 0.196 - 1.10 J/cm
0.367 - 2.06 ft-lb/in
Average value: 0.552 J/cm Grade Count:22
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Izod Impact, Notched 0.210 - 1.10 J/cm

@Temperature -40.0 - -20.0 °C
0.393 - 2.06 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.410 J/cm Grade Count:5
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Izod Impact, Notched 0.700 - 1.10 J/cm

@Temperature -40.0 - -40.0 °C
1.31 - 2.06 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.900 J/cm Grade Count:2
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..
Izod Impact, Notched 0.340 - 1.10 J/cm
0.637 - 2.06 ft-lb/in
Average value: 0.728 J/cm Grade Count:5
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.149 - 1.10 J/cm
0.280 - 2.06 ft-lb/in
Average value: 0.425 J/cm Grade Count:7
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..