Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.60 - 9.60 J/cm | 18.0 - 18.0 ft-lb/in | Average value: 9.60 J/cm Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.150 - 9.61 J/cm | 0.281 - 18.0 ft-lb/in | Average value: 1.16 J/cm Grade Count:343 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.481 - 9.61 J/cm | 0.900 - 18.0 ft-lb/in | Average value: 6.71 J/cm Grade Count:27 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.343 - 9.61 J/cm | 0.643 - 18.0 ft-lb/in | Average value: 6.22 J/cm Grade Count:215 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.320 - 9.60 J/cm | 0.599 - 18.0 ft-lb/in | Average value: 5.49 J/cm Grade Count:33 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 0.374 - 9.61 J/cm | 0.700 - 18.0 ft-lb/in | Average value: 1.15 J/cm Grade Count:24 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 6.94 - 9.61 J/cm | 13.0 - 18.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |