Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC THC-01-AS149031 Trans Blue Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid) 60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC M40060 Series High Density Polyethylene for Injection Molding Product Description: M40060 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 266 Specialty, Transparent
(discontinued **) A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and va.. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
3.37 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Izod Impact, Notched | >= 1.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 3.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Loxim 340 01HB Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: .. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched | 1.80 J/cm @Thickness 3.17 mm |
3.37 ft-lb/in @Thickness 0.125 in |
ASTM Test |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature -30.0 °C |
3.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 2417IG PA66, 20% glass fiber, DRY Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2417IG4 is used in all sectors of industries,.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180 |
Wellman Wellamid® GF43-66/6 XE-N 43% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
Toyobo Vylopet® EMC330K Glass Reinforced Polyester, Easy Molding Grade HB UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, c.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm @Temperature 23.0 °C |
3.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM 45% Glass Fiber Reinforced, High Strength.Information provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-G15 PTFE Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® T80 , Dimensional Stability PBT/ABS Alloy Dimensional StabilityInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.80 J/cm | 3.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |